For citation:
Galushkin N. E., Yazvinskaya N. N., Galushkin D. N. Investigation of the Causes of Thermal Run-away in Sealed Nickel-Cadmium Batteries. Electrochemical Energetics, 2012, vol. 12, iss. 4, pp. 208-211. DOI: 10.18500/1608-4039-2012-12-4-208-211, EDN: RDNCZJ
Investigation of the Causes of Thermal Run-away in Sealed Nickel-Cadmium Batteries
It is shown from analysis of charging current and voltage change on the terminals of sealed Ni-Cd battery at thermal runaway, that thermal runaway is accompanied by a new high-power electrochemical reaction, going at battery voltage of approximately 0.55 V.
1. Guo Y. // Encyclopedia of Electrochemical Power Sources, Vol. 4. Amsterdam: Elsevier, 2009. P. 241.
2. Коровин H. В. Химические источники тока: справочник. М.: МЭИ, 2003.
3. Галушкин Д. Н. И Электрохим. энергетика. 2008. Т. 8, № 4. С. 241.
4. Коровин Н. В. Электрохимическая энергетика. М.: Энергоатомиздат, 1991.
5. Галушкин Д. Н. И Электрохим. энергетика. 2006. Т. 6, № 2. С. 76.
6. Ni М. // Intern. J. of Hydrogen Energy. 2008 Vol. 33. P. 2337.
7. Wendt H. Electrochemical Hydrogen Technologies. Electrochemical production and combustion of hydrogen. Amsterdam: Elsevier, 1990.